2015年-2011年
Nakahira, A., Okimura, A., Hagiwara, Y., Nakanishi, T., Yokota, M., Inoue, M.
Development of a new type saw wire fixed diamond abrasive grains with solder and ni electroplating and its application to slicing of silicon and sapphire ingots
(2015) Funtai Oyobi Fummatsu Yakin/Journal of the Japan Society of Powder and Powder Metallurgy, 62 (12), pp. 559-566.
DOI: 10.2497/jjspm.62.559
Murakami, T., Noda, I., Ikeda, J., Nakahira, A.
Investigation of chemical state of vanadium at the interface between thermal sprayed hydroxyapatite coating and Ti-6Al-4V alloy substrate
(2015) Funtai Oyobi Fummatsu Yakin/Journal of the Japan Society of Powder and Powder Metallurgy, 62 (8), pp. 408-412.
DOI: 10.2497/jjspm.62.408
Kamitani, M., Kondo, M., Nakahira, A.
Experimental studies on ball milled wasted glasses and their self-hardening properties
(2015) Funtai Oyobi Fummatsu Yakin/Journal of the Japan Society of Powder and Powder Metallurgy, 62 (6), pp. 308-312.
DOI: 10.2497/jjspm.62.308
Iida, T., Sato, M., Numako, C., Nakahira, A., Kohara, S., Okubo, T., Wakihara, T.
Preparation and characterization of Silicalite-1 zeolites with high manganese contents from mechanochemically pretreated reactants
(2015) Journal of Materials Chemistry A, 3 (11), pp. 6215-6222.
DOI: 10.1039/c4ta06246a
Okada, K., Asakura, G., Tokudome, Y., Nakahira, A., Takahashi, M.
Macroporous titanate nanotube/TiO2 Monolith for fast and large-capacity cation exchange
(2015) Chemistry of Materials, 27 (5), pp. 1885-1891.
DOI: 10.1021/acs.chemmater.5b00184
Yamaguchi, T., Hagino, H., Michiyama, Y., Nakahira, A.
Sliding wear properties of Ti/TiC surface composite layer formed by laser alloying
(2015) Materials Transactions, 56 (3), pp. 361-366.
DOI: 10.2320/matertrans.M2014330
Murakami, T., Noda, I., Nakahira, A., Miyamoto, H., Mawatari, M.
Evaluation of the structure of Ag in thermal sprayed ag-containing hydroxyapatite coatings
(2015) Journal of the Ceramic Society of Japan, 123 (1440), pp. 667-671.
DOI: 10.2109/jcersj2.123.667
Takashima, K., Hoshino, M., Uesugi, K., Yagi, N., Matsuda, S., Nakahira, A., Osumi, N., Kohzuki, M., Onodera, H.
X-ray phase-contrast computed tomography visualizes the microstructure and degradation profile of implanted biodegradable scaffolds after spinal cord injury
(2015) Journal of Synchrotron Radiation, 22 (1), pp. 136-142.
DOI: 10.1107/S160057751402270X
2014年
Yamaguchi, T., Hagino, H., Takemura, M., Nakahira, A.
Formation and microstructural characterization of Ti/TiC surface composite layer by laser alloying treatment using graphite powder
(2014) Funtai Oyobi Fummatsu Yakin/Journal of the Japan Society of Powder and Powder Metallurgy, 61 (10), pp. 481-486.
DOI: 10.2497/jjspm.61.481
Yagi, S., Nakatsuji, K., Satake, Y., Nakahira, A., Anpo, M.
Thermodynamic consideration on degradation of humic acids by electrolysis
(2014) Electrochemistry, 82 (1), pp. 19-24.
DOI: 10.5796/electrochemistry.82.19
Tokudome, Y., Okada, K., Nakahira, A., Takahashi, M.
Switchable and reversible water adhesion on superhydrophobic titanate nanostructures fabricated on soft substrates: Photopatternable wettability and thermomodulatable adhesivity
(2014) Journal of Materials Chemistry A, 2 (1), pp. 58-61.
DOI: 10.1039/c3ta13536e
Sato, M., Nakahira, A.
Preparation of iron doped hydroxyapatite microsphere by mist process
(2014) Materials Transactions, 55 (10), pp. 1536-1539.
DOI: 10.2320/matertrans.Y-M2014830
Yamaguchi, T., Hagino, H., Takemura, M., Nakahira, A.
Microstructure of MC-Fe composite layer on carbon steel by laser surface alloying
(2014) Journal of Laser Micro Nanoengineering, 9 (2), pp. 83-87.
DOI: 10.2961/jlmn.2014.02.0001
Nakahira, A., Nishimoto, H., Hamada, Y., Yamasaki, Y.
Synthesis and characterization of dense mesoporous alumina
(2014) Key Engineering Materials, 616, pp. 252-257.
DOI: 10.4028/www.scientific.net/KEM.616.252
Nakahira, A., Yamamoto, S., Onodera, H.
Synthesis and evaluation of Fe nanowire and nanorod by electro-chemical process
(2014) Key Engineering Materials, 616, pp. 237-241.
DOI: 10.4028/www.scientific.net/KEM.616.237
Nakahira, A., Kawabe, Y., Yamamoto, S., Onodera, H.
Synthesis of S and N Co-doped mesoporous titanium oxide by anodization processs
(2014) Key Engineering Materials, 616, pp. 72-76.
DOI: 10.4028/www.scientific.net/KEM.616.72
Tsujiguchi, M., Kobashi, T., Utsumi, Y., Kakimori, N., Nakahira, A.
Synthesis of FAU zeolite from aluminoborosilicate glass and elution behavior of glass components
(2014) Journal of the Ceramic Society of Japan, 122 (1421), pp. 104-109.
DOI: 10.2109/jcersj2.122.104
Tsujiguchi, M., Kobashi, T., Utsumi, Y., Kakimori, N., Nakahira, A.
Synthesis of zeolite a from aluminoborosilicate glass used in glass substrates of liquid crystal display panels and evaluation of its cation exchange capacity
(2014) Journal of the American Ceramic Society, 97 (1), pp. 114-119.
DOI: 10.1111/jace.12671
Tsujiguchi, M., Kobashi, T., Oki, M., Utsumi, Y., Kakimori, N., Nakahira, A.
Synthesis and characterization of zeolite A from crushed particles of aluminoborosilicate glass used in LCD panels
(2014) Journal of Asian Ceramic Societies, 2 (1), pp. 27-32.
DOI: 10.1016/j.jascer.2013.12.005
Kamitani, M., Tagami, T., Fukaya, T., Kondo, M., Hiki, T., Nakahira, A.
Synthesis of A- Type zeolite from flat glass recycle by hydrothermal treatments and its evaluation
(2014) Key Engineering Materials, 616, pp. 183-187.
DOI: 10.4028/www.scientific.net/KEM.616.183
Kamitani, M., Tagami, T., Kondo, M., Hiki, T., Wakihara, T., Nakahira, A.
Fabrication and evaluation of hybrid materials from A-zeolite and ground glass powders for vitrified radioactive waste
(2014) Journal of the Ceramic Society of Japan, 122 (1422), pp. 151-155.
DOI: 10.2109/jcersj2.122.151
Iida, T., Sato, M., Liu, Z., Numako, C., Nakahira, A., Okubo, T., Wakihara, T.
Synthesis of MCM-41 with high manganese content by mechanochemical pretreatment of the starting materials
(2014) Chemistry Letters, 43 (8), pp. 1346-1348.
DOI: 10.1246/cl.140340
Shitara, K., Murata, H., Watanabe, K., Kojima, C., Sumida, Y., Nakamura, A., Nakahira, A., Tanaka, I., Matsunaga, K.
Cytotoxicity of stoichiometric hydroxyapatites with different crystallite sizes
(2014) Journal of Asian Ceramic Societies, 2 (1), pp. 64-67.
DOI: 10.1016/j.jascer.2014.01.002
2013年
Kojima, C., Watanabe, K., Nagayasu, T., Nishio, Y., Makiura, R., Nakahira, A.
Preparation of hydroxyapatite-decorated poly(lactide-co-glycolide) microspheres for paclitaxel delivery
(2013) Journal of Nanoparticle Research, 15 (12), .
DOI: 10.1007/s11051-013-2098-z
Yamaguchi, T., Hagino, H., Takemura, M., Hasegawa, Y., Michiyama, Y., Nakahira, A.
Microstructure of FeTiC composite surface layer on carbon steel formed by laser alloying process
(2013) Materials Transactions, 54 (9), pp. 1755-1759.
DOI: 10.2320/matertrans.MAW201304
Yoshida, K., Toyoura, K., Matsunaga, K., Nakahira, A., Kurata, H., Ikuhara, Y.H., Sasaki, Y.
Atomic sites and stability of Cs+ captured within zeolitic nanocavities
(2013) Scientific Reports, 3, art. no. 2457, .
DOI: 10.1038/srep02457
Tsujiguchi, M., Kobashi, T., Kanbara, J., Utsumi, Y., Kakimori, N., Nakahira, A.
Synthesis and characterization of zeolite from glass by hydrothermal processing
(2013) Materials Science Forum, 761, pp. 91-94.
DOI: 10.4028/www.scientific.net/MSF.761.91
Akola, J., Kohara, S., Ohara, K., Fujiwara, A., Watanabe, Y., Masuno, A., Usuki, T., Kubo, T., Nakahira, A., Nitta, K., Uruga, T., Richard Weber, J.K., Benmore, C.J.
Network topology for the formation of solvated electrons in binary CaO-Al2O3 composition glasses
(2013) Proceedings of the National Academy of Sciences of the United States of America, 110 (25), pp. 10129-10134.
DOI: 10.1073/pnas.1300908110
Tsujiguchi, M., Kobashi, T., Kanbara, J., Utsumi, Y., Kakimori, N., Nakahira, A.
Synthesis of zeolite from glass
(2013) Zairyo/Journal of the Society of Materials Science, Japan, 62 (6), pp. 357-361.
DOI: 10.2472/jsms.62.357
Watanabe, K., Nishio, Y., Makiura, R., Nakahira, A., Kojima, C.
Paclitaxel-loaded hydroxyapatite/collagen hybrid gels as drug delivery systems for metastatic cancer cells
(2013) International Journal of Pharmaceutics, 446 (1-2), pp. 81-86.
DOI: 10.1016/j.ijpharm.2013.02.002
Sato, M., Nakahira, A.
Influence of Fe addition to hydroxyapatite by aqueous solution process
(2013) Journal of the Ceramic Society of Japan, 121 (1413), pp. 422-425.
DOI: 10.2109/jcersj2.121.422
Sato, M., Nakahira, A.
Influence of Fe addition to hydroxyapatite by hydrothermal process
(2013) Journal of the Ceramic Society of Japan, 121 (1415), pp. 559-562.
DOI: 10.2109/jcersj2.121.559
Okada, K., Takamatsu, Y., Tokudome, Y., Nakahira, A., Takahashi, M.
Highly oriented growth of titanate nanotubes (TNTs) in micro and confinement spaces on sol-gel derived amorphous TiO2 thin films under moderate hydrothermal condition
(2013) Journal of Sol-Gel Science and Technology, 65 (1), pp. 36-40.
DOI: 10.1007/s10971-012-2685-y
Katayama, H., Banba, N., Sugimura, Y., Tatsumi, M., Kusakari, S.-I., Oyama, H., Nakahira, A.
Subcellular compartmentation of strontium and zinc in mulberry idioblasts in relation to phytoremediation potential
(2013) Environmental and Experimental Botany, 85, pp. 30-35.
DOI: 10.1016/j.envexpbot.2012.06.001
2012年
Onoki, T., Nakahira, A., Tago, T., Hasegawa, Y., Kuno, T.
Novel low temperature processing techniques for apatite ceramics and chitosan polymer composite bulk materials and its mechanical properties
(2012) Applied Surface Science, 262, pp. 263-266.
DOI: 10.1016/j.apsusc.2012.09.031
An, S.-H., Matsumoto, T., Miyajima, H., Nakahira, A., Kim, K.-H., Imazato, S.
Porous zirconia/hydroxyapatite scaffolds for bone reconstruction
(2012) Dental Materials, 28 (12), pp. 1221-1231.
DOI: 10.1016/j.dental.2012.09.001
Suzuki, N., Huang, Y.-T., Nemoto, Y., Nakahira, A., Yamauchi, Y.
Highly densified mesoporous bulk silica prepared with colloidal mesoporous silica nanoparticles toward a new low-κ material
(2012) Chemistry Letters, 41 (11), pp. 1518-1519.
DOI: 10.1246/cl.2012.1518
Inoue, M., Kawagishi, S., Hagihara, Y., Tomiyoshi, T., Inoue, H., Murata, Y., Yokota, M., Nakahira, A.
Development of a new type saw wire fixed diamond abrasive grains with solder and Ni electroplating and its application to slicing of sapphire ingots
(2012) Funtai Oyobi Fummatsu Yakin/Journal of the Japan Society of Powder and Powder Metallurgy, 59 (8), pp. 465-472.
DOI: 10.2497/jjspm.59.465
Okada, K., Tokudome, Y., Falcaro, P., Takamatsu, Y., Nakahira, A., Takahashi, M.
Titanate nanofunnel brushes: Toward functional interfacial applications
(2012) Chemical Communications, 48 (49), pp. 6130-6132.
DOI: 10.1039/c2cc32081a
Inoue, M., Ohtani, Y., Shimada, H., Tomiyoshi, T., Inoue, H., Murata, Y., Yokota, M., Nakahira, A.
Development of diamond saw wire using Pb-free solder as fixing material and its application to slicing of sapphire ingot
(2012) Funtai Oyobi Fummatsu Yakin/Journal of the Japan Society of Powder and Powder Metallurgy, 59 (5), pp. 227-232.
DOI: 10.2497/jjspm.59.227
2011年
Wakihara, T., Ihara, A., Inagaki, S., Tatami, J., Sato, K., Komeya, K., Meguro, T., Kubota, Y., Nakahira, A.
Top-down tuning of nanosized ZSM-5 zeolite catalyst by bead milling and recrystallization
(2011) Crystal Growth and Design, 11 (11), pp. 5153-5158.
DOI: 10.1021/cg201078r
Matsumoto, T., Uddin, M.H., An, S.H., Arakawa, K., Taguchi, E., Nakahira, A., Okazaki, M.
Modulation of nanotube formation in apatite single crystal via organic molecule incorporation
(2011) Materials Chemistry and Physics, 128 (3), pp. 495-499.
DOI: 10.1016/j.matchemphys.2011.03.045
Inoue, M., Higashi, T., Onoki, T., Yokota, M., Murata, Y., Nakahira, A.
Wettability, interfacial reaction and joint strength between low melting ag based brazing alloy and some industrial metal plates
(2011) Funtai Oyobi Fummatsu Yakin/Journal of the Japan Society of Powder and Powder Metallurgy, 58 (7), pp. 407-411.
DOI: 10.2497/jjspm.58.407
Suehiro, T., Tada, T., Waku, T., Tanaka, N., Hongo, C., Yamamoto, S., Nakahira, A., Kojima, C.
Temperature-dependent higher order structures of the (Pro-Pro-Gly) 10-modified dendrimer
(2011) Biopolymers, 95 (4), pp. 270-277.
DOI: 10.1002/bip.21576